It will then be left to dry slowly in preparation for the first firing - as these pieces are doing. The pieces are quite fragile at this point and have to be handled with care.
Once dry, these pieces will be loaded in the kiln and fired to about 1960 degrees F. This takes approximately 13 hours. The kiln will be allowed completely cool before being opened - about a day and a half later.